Introduction and Background

  • Destin visits Kodak plant in Rochester, NY to understand film manufacturing process
  • Analog film photography experiencing huge comeback - secondhand camera prices through roof
  • Question: Are they manufacturing new film or selling old stockpile?
  • Three-part video series covering complete manufacturing process
    • Part 1: Support (polyester base)
    • Part 2: Light sensitivity (emulsion coating)
    • Part 3: Packaging (in darkness)
  • No Kodak sponsorship - purely educational visit

Kodak Plant Overview

  • Located at Kodak Park, Rochester NY - originated 1891
  • Building 1 was first building constructed
  • Steam generation plant for power
  • Photographic film only small percentage of total business
  • Historic campus with old brickwork, pipes, textures
  • Matt Stoffel (IT manager) - third generation "Kodecker"
  • Family legacy: father, grandfather, aunts, uncles, grandmother all worked there

Estar Film Base Manufacturing Introduction

  • Estar = Kodak trade name for PET (polyethylene terephthalate) polyester
  • Continuous biaxial orienting process - stretches in two dimensions
  • Advantages over acetate:
    • Higher strength and longevity
    • Recyclable
    • Much higher tensile strength
  • Disadvantage: May break camera before film fails
  • Motion picture origination still uses acetate (intentional weak point)
  • Projector film uses Estar for durability through hundreds of showings

Raw Material Processing

  • Railway cars deliver PET pellets - one car lasts 2 days
  • First step: Mechanical grinding
    • 250 horsepower motors
    • 10,000 pounds/hour capacity
    • Converts pellets to fine powder for increased surface area
  • Pneumatic conveyor transports powder 100+ feet up to 300,000 pound storage tanks

Fluidized Polymer Reactors (FPRs)

  • Purpose: Solid stating process - removes moisture
  • Target: 5 parts per million moisture by weight
  • Process details:
    • 10,000 pound batches (older reactors)
    • Two 20,000 pound reactors (currently running)
    • Fluidized bed with dry nitrogen flow
    • Distribution plate with tiny holes creates ocean-like waves
    • 7 PSI pressure
    • Internal and external heating coils
  • Temperature control critical for uniform processing
  • Nitrogen recirculation system with glycol scrubbers
  • Closed-loop nitrogen system (expensive to waste)
  • All stainless steel construction - no aluminum or silicon allowed

Quality Control and Screening

  • Intrinsic viscosity (IV) testing correlates to moisture content
  • Tiny Olsen machine measures viscosity of melted samples
  • Screening process removes oversized particles
  • Particle size distribution maintained within acceptable range

Melt Extrusion Process

  • 200 horsepower motor with gearbox
  • Screw specifications:
    • ~40 feet long
    • 30 RPM rotation speed
    • Multiple sections with varying flight depths
  • Process stages:
    • Feed throat accepts powder
    • Frictional heat melts material (540°F)
    • Pressure builds to 1,200 PSI
    • Vacuum extraction section removes volatile gases
    • Final pressurization before exit
  • Jacketed piping maintains uniform temperature
  • Two-screw system: primary screw does heavy lifting, secondary metering screw provides fine control

Filtration System

  • Molten polymer filtered through 5-10 micron stainless steel mesh
  • Filter sticks cleaned and reused
  • Critical for optical clarity in final product

Casting Wheel Process

  • Large polished wheel (mirror finish)
  • Molten material (540°F) extruded at 12 o'clock position
  • Vacuum applied to ensure adhesion and uniformity
  • Cooling from 540°F to 135°F during rotation
  • Rapid cooling prevents crystalline structure (maintains optical clarity)
  • Material emerges very thick (~1/8 inch) moving slowly
  • 4,400 pounds/hour throughput (without reuse)

Coating Stations

  • Multiple coating applications possible:
    • Primer for photosensitive layer adhesion
    • Anti-static layers
    • Conductive layers
    • Gelatin coatings
  • Combustible solvent storage room with explosion-proof design
  • Electrically grounded containers prevent static discharge
  • Patrick (engineer) manages coating preparation systems

Stretching Process - Drafting

  • Material has thick ribs on edges for gripping
  • Machine direction stretching (drafting):
    • Heated air chambers
    • Edge rollers grip ribs
    • Tension-controlled stretching
    • Thickness reduces from 107 to 50 thousandths of inch
    • Speed increases 3.5x during stretch
    • Stretch ratio approximately 3.5:1
  • Temperature and tension control critical for consistent stretch point
  • Cooling section follows stretching

Stretching Process - Tentering

  • Transverse direction stretching using chain-mounted clips
  • ~1,000 clips on continuous chains
  • Process sequence:
    • Cam mechanism closes clips on film edges
    • Width increases from 16.5" to 60" (full width)
    • Heat application enables uniform stretching
    • Heat set at higher temperature locks molecular structure
    • Controlled cooling and relaxation
    • Clips release and return to start position

Molecular Orientation

  • Biaxial stretching aligns polymer molecules
  • Transforms random "spaghetti-like" structure to organized lengthwise and widthwise alignment
  • Heat set process locks crystalline structure
  • Results in tough PET properties

Final Processing

  • Edge trimming removes ribs (recycled back to process)
  • Nuclear thickness gauge provides real-time feedback
  • Thickness measurement feeds back to die heaters at casting wheel
  • Sophisticated closed-loop control system
  • Additional coating stations available for full-width applications
  • Defect scanning with laser and CCD cameras
  • Knurling/embossing capabilities (Sharon holds patents)
  • Slitting to various widths possible

Accumulator System

  • Solves problem of continuous production during roll changes
  • Series of pulleys that can spread apart
  • Equation: Production velocity = Accumulator velocity + Spool velocity
  • Allows stopping/starting spool while maintaining line speed
  • Demonstration showed practical application

Final Winding and Quality Control

  • Line speed: 260 feet/minute at 5,500+ feet per roll
  • Steve (21-22 years experience) operates winding station
  • Accumulator percentage indicates safety margin (lower is better)
  • Knife cutting system with safety light curtains
  • Sample collection for quality testing:
    • Quality samples
    • Keeping samples (stored for customer complaints)
  • Roll removal using specialized carts and torque chucks
  • Final packaging in wooden caskets for shipping

Workforce Dynamics

  • Impressive mentorship between experienced and younger employees
  • Older generation sharing knowledge and work ethic
  • Younger generation bringing tech-savvy approach
  • Encouraging example of American manufacturing partnership
  • Pride in craftsmanship and continuous improvement

TwinMind

Get summaries like this for your own meetings

TwinMind takes notes in the background during meetings, lectures, and calls, then writes the summary for you.

Free plan to get started

No bot joins your calls

Phone, desktop & Chrome apps

Your next meeting, summarized like this

TwinMind listens in the background and turns meetings, lectures, and calls into searchable notes you can chat with. Start free.

Available on phone, desktop & Chrome

Your next meeting, summarized like this

TwinMind listens in the background and turns meetings, lectures, and calls into searchable notes you can chat with. Start free.

Available on phone, desktop & Chrome

Your next meeting, summarized like this

TwinMind listens in the background and turns meetings, lectures, and calls into searchable notes you can chat with. Start free.

Available on phone, desktop & Chrome